Abstract: <正> 我厂碱性平炉冶炼的38CrMoA1钢,在锻造时产生裂纹,其纵向断口是变形能力较差、呈致密而较平坦的灰白色大块岩石形异状断口,使横向机械性能(尤其是δ、φ、α_k值)显著降低。通过对异状断口二次复型进行了大量透射电子显微镜观察,发现异状断口区存在大量非金属夹杂引起沿晶断裂;经选区电子衍射分析,确定其为AIN夹杂。这